Welding Instruction |
|||||||||||
(1) Dry the electrodes at 70-100°C for 30-60 minutes before use. (2) Clean up the contaminations on the steel to prevent porosity. (3) Preheat temperature should be above 150°C for multi-layer welding of low alloy steel or high carbon steel. (4) Welding parameter and operating technique must be carefully chosen to prevent slag inclusion in narrow gaps welding. |
|||||||||||
Typical Chemical Composition of Weld Metal (wt. %) |
|||||||||||
C |
Si |
Mn |
Cr |
||||||||
0.150 |
0.50 |
0.58 |
1.25 |
||||||||
Typical Hardness of Weld Metal |
|||||||||||
Hardness Condition |
Vicker’s hardness (HV) |
Rockwell’s hardness (HRC) |
Shore’s hardness (HS) |
||||||||
Interpass temp. Temp. ≤150°C |
260 |
24 |
37 |
||||||||
Continuous build-up |
220 |
16 |
33 |
||||||||
Size and Suggested Operating Range (AC or DC+) |
|||||||||||
Diameter x Length(mm) |
2.0x250 |
2.6x300 |
3.2x350 |
4.0x350 |
5.0x350 |
||||||
Amp |
35~55 |
50~85 |
80~120 |
100~150 |
140~200 |