Welding Position
|
|||||||||||||||
All Positions
|
|||||||||||||||
TypicalChemical Composition of Weld Metal (wt. %)
|
|||||||||||||||
C
|
Si
|
Mn
|
P
|
S
|
Cr
|
Ni
|
Mo
|
||||||||
0.100
|
0.46
|
1.68
|
0.015
|
0.010
|
26.84
|
21.06
|
2.42
|
||||||||
TypicalMechanical Properties of Weld Metal
|
|||||||||||||||
Tensile Strength
N/mm2(kgf/mm2)
|
Yield Strength
N/mm2(kgf/mm2)
|
Elongation
%
|
|||||||||||||
590(60.2)
|
430(43.8)
|
36
|
|||||||||||||
Size and SuggestedOperating Range (AC or DC+)
|
|||||||||||||||
Diameter x Length (mm)
|
2.0x250
|
2.6x300
|
3.2x350
|
4.0x350
|
5.0x350
|
||||||||||
Amp
|
F/H-Fillet
|
35~55
|
50~85
|
80~120
|
100~150
|
140~200
|
|||||||||
V-up/OH
|
30~50
|
45~85
|
70~110
|
90~135
|
—
|