Welding Instruction |
|||||||||||||||
(1) Use Ar blend with 1~2%O2 for high current, spray transfer welding. (2) Use Ar blend with 1~2%CO2 for low current, short-circuit transfer welding. |
|||||||||||||||
Typical Chemical Composition of Weld Metal (wt %) (Shielding Gas : Ar+2%O2) |
|||||||||||||||
C |
Si |
Mn |
P |
S |
Cr |
Ni |
|||||||||
0.06 |
0.40 |
1.36 |
0.02 |
0.02 |
19.56 |
10.23 |
|||||||||
Typical Mechanical Properties of Weld Metal (Shielding Gas : Ar+2%O2) |
|||||||||||||||
Tensile Strength Yield Strength N/mm2(kgf/mm2) N/mm2(kgf/mm2) |
Elongation % |
||||||||||||||
560 370 |
45 |
||||||||||||||
|
|||||||||||||||
|
Size and Suggested Operating Range (DC+) |
||||||||||||||
|
Diameter (mm) Operating range |
0.8 |
0.9 |
1.0 |
1.2 |
1.4 |
1.6 |
||||||||
|
Ar+1~2%CO2 |
Amp |
— |
60~140 |
80~160 |
100~210 |
— |
— |
|||||||
|
Volt |
— |
15~21 |
16~22 |
17~22 |
— |
— |
||||||||
|
Ar+1~2%O2 |
Amp |
— |
170~260 |
180~280 |
200~300 |
210~320 |
220~330 |
|||||||
|
Volt |
— |
24~30 |
24~30 |
24~30 |
24~32 |
24~32 |